Figure 8 | Scientific Reports

Figure 8

From: Electrical conduction and noise spectroscopy of sodium-alginate gold-covered ultrathin films for flexible green electronics

Figure 8

Comparison between DC and AC properties of metallic samples. The temperature dependencies of the normalized resistance R/R300K (a) and of the Noise Level NL (b) are shown for PMMA on glass (squares), SA on glass (circles), and SA free-standing (triangles) films. The typical characteristics of metallic compounds are observed, especially regarding the very low noise measured in the whole investigated temperature range.