Figure 2 | Scientific Reports

Figure 2

From: Probing intergranular mixed transgranular stress corrosion cracking under the high constant load

Figure 2

Two- and three-dimensional fracture surface morphologies of the upper half part of an initially-fractured specimen subjected to the chloride-solution immersion of about 10 h. a Two-dimensional SEM morphology. b Three-dimensional XCT morphology consisting of three fracture surfaces marked by ‘1–3’ and a tomographic slice labeled by a dotted rectangle.