Figure 8

SEM images showing fracture surfaces of HIPS after tensile test at (a) ×55, (c) ×500, (e) ×5000 and after notched tensile test at (b) ×25, (d) ×500 and (f) ×5000.
SEM images showing fracture surfaces of HIPS after tensile test at (a) ×55, (c) ×500, (e) ×5000 and after notched tensile test at (b) ×25, (d) ×500 and (f) ×5000.