Figure 10
From: Comparison between bearing strengths of molded-in and machined holes of GFR/PP composites

SEM images of a cross-section of the fractured zone of specimens; (a) 10 wt% GF (12 mm initial length) + 90 wt% PP and (b) 30 wt% GF (12 mm initial length) + 70 wt% PP.