Figure 6
From: Study of wide bandgap SnOx thin films grown by a reactive magnetron sputtering via a two-step method

TOF-SIMS profiles for the best conductive sample (SnOx deposited at 250 °C, at 1.5% O2/Ar ratio, and annealed under vacuum at 400 °C).