Figure 3
From: On the analyses of carbon atom diffused into grey cast iron during carburisation process

Diffusion of carbon atoms into the surface of grey cast iron at 900° for 90 min.
From: On the analyses of carbon atom diffused into grey cast iron during carburisation process

Diffusion of carbon atoms into the surface of grey cast iron at 900° for 90 min.