Figure 8

Power maps with different H of (a) 50 nm, (b) 100 nm, (c) 150 nm and (d) 200 nm respectively. In the simulation, \(L_{in}\) is 10 \(\upmu \)m and D is 300 nm. (e) Coupling efficiency versus different detunings.
Power maps with different H of (a) 50 nm, (b) 100 nm, (c) 150 nm and (d) 200 nm respectively. In the simulation, \(L_{in}\) is 10 \(\upmu \)m and D is 300 nm. (e) Coupling efficiency versus different detunings.