Figure 6

Growth curves of depolarized light intensity (DLI) with/without applied shear history during cooling at 10 °C min−1. The shear history was applied from 170 °C (left) and 180 °C (right) to 130 °C at 10 and 50 s−1.
Growth curves of depolarized light intensity (DLI) with/without applied shear history during cooling at 10 °C min−1. The shear history was applied from 170 °C (left) and 180 °C (right) to 130 °C at 10 and 50 s−1.