Table 1 Analysis of the surface area of fabricated Nitrogen-doping activated carbons.
Analysis method | Sample entry | NDAC600 | NDAC700 | NDAC800 | |
|---|---|---|---|---|---|
AC yield | (%) | 25.03 | 25.757 | 21.545 | |
BET | as, BET (m2∕g) | SBET (m2/g) | 553.63 | 783.78 | 727.34 |
Vm (cm3/g) | Vm (cm3 (STP)/g) | 124.2 | 180.08 | 167.11 | |
Mean pore diameter | Dp (nm) | 2.0584 | 2.0194 | 1.9668 | |
Volume of total pore | VT (cm3/g) | 0.2849 | 0.3957 | 0.3576 | |
t-plot | a1–a2 | Smi (m2/g) | 640.649 | 894.315 | 864.64 |
V2 | Vmi (cm3/g) | 0.2441 | 0.3515 | 0.3193 | |
2t | (nm) | 0.7573 | 0.7813 | 0.7341 | |
MP | a1-a2 | (m2 ∕g) | 604.981 | 851.67 | 810.177 |
Vp | (cm3∕g) | 0.2536 | 0.3626 | 0.3337 | |
BJH ads | Vp | (cm3/g) | 0.0822 | 0.109 | 0.0862 |
ap | (m2/g) | 76.743 | 109.49 | 84.85 | |
BJH des | Vp | Vme (cm3/g) | 0.0512 | 0.0609 | 0.0499 |
ap | Sme (m2/g) | 32.867 | 40.58 | 32.378 | |