Crack path crystallography of (a) δ-FG and (b) CG in the presence of H at ΔK = 10 MPa m1/2: ECC images for overall aspects are in (a-1) and (b-1). Inverse pole figure (IPF) maps with respect to the loading axis at the regions A–C for δ-FG and D–F for CG are in (a-3–a-5,b-3–b-5) with {111} plane traces.