Table 3 Values of cell viability of the undoped and 0.6 mol% ZnO doped borate glasses with different concentrations of each glass.
From: Structural, optical, and cytotoxicity studies of laser irradiated ZnO doped borate bioactive glasses
Glass | Cell viability % | |||||
|---|---|---|---|---|---|---|
50 | 25 | 12.5 | 6.25 | 3.125 | 1.5625 | |
Base | 89.28877 | 95.11568 | 96.11568 | 98.9709 | 101.1705 | 102.6281 |
88.94773 | 94.14567 | 95.74464 | 97.34362 | 100.3436 | 103.1722 | |
0.6 mol% ZnO | 74.72151 | 82.26221 | 87.97601 | 90.48843 | 93.91602 | 95.45844 |
83.69494 | 87.89289 | 91.52014 | 97.8329 | 99.11911 | 101.8029 | |