Table 2 XRF results of FFA used in this study.
From: Mixed Micromax and hematite-based fly ash geopolymer for heavy-weight well cementing
Oxide | Percentage (%) |
---|---|
SiO2 | 55.92 |
Al2O3 | 29.54 |
CaO | 5.49 |
Fe2O3 | 4.93 |
TiO2 | 1.91 |
K2O | 1.66 |
SO3 | 0.39 |
Others | 0.17 |
From: Mixed Micromax and hematite-based fly ash geopolymer for heavy-weight well cementing
Oxide | Percentage (%) |
---|---|
SiO2 | 55.92 |
Al2O3 | 29.54 |
CaO | 5.49 |
Fe2O3 | 4.93 |
TiO2 | 1.91 |
K2O | 1.66 |
SO3 | 0.39 |
Others | 0.17 |