Figure 7
From: Trimming flow, plasticity, and mechanical properties by cubic silsesquioxane chemistry

Optical microscopy images of tensile specimens’ cross section after fracture. (A1, A2) neat PLA, (B) OSS-8TMOS, (C) OSS-2OD-6TMOS, (D) OSS-4OD-4TMOS, (E) OSS-5OD-3TMOS, (F) OSS-8OD. For samples (B–F), 1 represents 0.5% additive loading, 2–1%, and 3–2.5%.