Table 2 Ultimate force, stress, and break distance from mechanical compression.
From: Impact of micro/nano cadmium oxide on shielding properties of cement–ball clay matrix
Parameter | Sample | ||||
---|---|---|---|---|---|
CS | CB-m CdO 8.3% | CB-n CdO 8.3% | CB-m CdO 16.7% | CB-n CdO 16.7% | |
Ultimate force (N) | 115.67 | 712.65 | 884.12 | 692.27 | 1101.00 |
Ultimate stress (MPa) | 2.35 | 1.45 | 1.80 | 1.41 | 2.24 |
Break distance (mm) | 4.84 | 3.02 | 5.56 | 5.64 | 2.67 |