Figure 8
From: Corrosion suppression and strengthening of the Al-10Zn alloy by adding silica nanorods

SEM images after the corrosion test before and after different aging temperatures of AZ and AZS with a scale bar of 100 µm.
From: Corrosion suppression and strengthening of the Al-10Zn alloy by adding silica nanorods
SEM images after the corrosion test before and after different aging temperatures of AZ and AZS with a scale bar of 100 µm.