Table 2 The grain size calculations of the Al grains of the composites before and after aging temperatures (423, 443, and 463 K).
From: Corrosion suppression and strengthening of the Al-10Zn alloy by adding silica nanorods
Grain size (µm) | ||||
---|---|---|---|---|
Sample | As-cast | 423 K | 443 K | 463 K |
AZ | 190 | 102 | 77 | 90 |
AZS | 170 | 80 | 59 | 65 |