Table 3 σUTS, σy, and σFrature, of the composites.

From: Corrosion suppression and strengthening of the Al-10Zn alloy by adding silica nanorods

423 K

443 K

463 K

Sample

σUTS

MPa

σy

MPa

σFracture

MPa

σUTS

MPa

σy

MPa

σFracture

MPa

σUTS

MPa

σy

MPa

σFracture

MPa

AZ

151.8

135.4

139

278

238

263.9

177

166

177.6

AZS

250

218.7

241.5

482.6

391

472.9

204.9

174.5

186.5