Table 1 Rate constant and activation parameters of catalytic degradation of AO7 by [Co(II) TPHPP] -Cs / GO nanocomposite with H2O2.
Temperature (°K) | Kobs (min−1) | ΔΓ# (k J μοl−1) | Ea (k J mol−1) | ΔΗ# (k J μοl−1) | ΔΣ# (J mοl−1 Κ−1) |
---|---|---|---|---|---|
289 | 0.006 | 85.79 | |||
313 | 0.011 | 88.45 | 35.5 | 35.5 | − 1.77 × 102 |
321 | 0.013 | 89.87 | |||
328 | 0.025 | 91.11 |