Table 4 Weight loss (mg) and wear rate (mg/s) at different applied loads, i.e., 20 and 40 N for all prepared samples.

From: Role of Ti3AlC2 MAX phase in regulating biodegradation and improving electrical properties of calcium silicate ceramic for bone repair applications

Samples name

Weight loss (mg)

 

Wear rate (mg/s)

 
 

20 N

40 N

20 N

40 N

CHM1

0.9814

1.1658

0.0016

0.0019

CHM2

1.3120

1.4586

0.0022

0.0024

CHM3

1.6013

1.7222

0.0027

0.0029

CHM4

0.9643

1.0046

0.0016

0.0017

CHM5

0.6582

0.6164

0.0011

0.0010