Table 5 Heating characteristics of the various nanoalloys (f = 332 kHz and H0 = 170 oe).

From: Tuning the physical properties of ternary alloys (NiCuCo) for in vitro magnetic hyperthermia: experimental and theoretical investigation

Samples

Maximum temperature (°C)

Time needed to reach hyperthermia temperature 42 °C (min)

Ms (emu/g)

SAR (W/g)

Ni35Cu30Co35

52.65

6.47

42.63

76.358

Ni25Cu50Co25

50.07

7.67

21.49

51.02

Ni15Cu70Co15

40.42

Not reaching

4.73

16