Table 3 EOS parameters of Rh measured and calculated in different experiments. The volume \(V_0\), the bulk modulus \(K_0\) and its pressure derivative \(K'\) are listed. Experimental methods and EoS formulation are specified. Notice that the parameters used where obtained not always using the same equation of states. More information on the equations of states can be found in the corresponding references.For completeness, we have also included the references for the pressure scales used in each work.

From: Thermal equation of state of rhodium characterized by XRD in a resistively heated diamond anvil cell

Reference

\(\mathbf {V_0}\)\(^3\))

\(\mathbf {K_0}\) (GPa) \(\mathbf {K'}\)

PTM

Pressure gauge

EoS

Method

Pressure Range (GPa)

This study

55.046(16)

251(3), 5.7(2)

He

Au28

Vinet

AD-XRD DAC

0-55

This study

55.045(15)

252(3), 5.5(2)

He

Au28

BM3

AD-XRD DAC

0-55

14

55.056(8)

258(3), 5.36(9)

Bi

Bi30

AP2

AD-XRD DAC

0-180

13

55.062(63)

241.3(65), 5.34(24)

Ne

Tungsten31

Vinet

AD-XRD DAC

0-60

12

54.92(7)

301(9), 3.1(2)

Ne

Ruby32

BM3

AD-XRD DAC

0-65

11

54.952

270.0, 4.756

Ne

Cu

BM3

AD-XRD DAC

31-83

10

55.008(4)

269(8), 4.5(1)

   

Single-shock

0-212 GPa

33

 

264(1)

   

ultrasound

 

34

54.83

299.4, 4.9

   

Theo

0-300 GPa

This study

53.8

299, 4.9

  

BM3

Theo-DFT

0-140