From: In-situ synthesis and integration of gold nanoparticles into 3D printed optical fiber probes

Fig. 3

(A) Reflection mode measurement setup, (B) transmission mode measurement setup, (C) reflection spectra from the single material (High-AuNPs) OFPs under white light (the number indicates dipping time 30 s, 1 min, 2 min, 5 min, and 10 min respectively), (D) reflection at wavelengths of 500, 550, and 600 nm (High-AuNPs), (E) reflection spectra from the single material (low-AuNPs) OFPs under white light, (F) reflection at wavelengths 500, 550, and 600 nm (low-AuNPs), (G) transmission spectra from the single material (low-AuNPs) OFPs under white light, (H) transmission at wavelengths 500, 550, and 600 nm (low-AuNPs), (I) transmission spectra from the single material (high-AuNPs) OFPs under white light, and (J) transmission at wavelengths 500, 550, and 600 nm (high-AuNPs).