Fig. 5

Galvanostatic charge of the IntPB: (a-e) Charging of the prepared NbWO||Li cell at constant voltage at 80, 50, -60, -80, -105 oC.
Galvanostatic charge of the IntPB: (a-e) Charging of the prepared NbWO||Li cell at constant voltage at 80, 50, -60, -80, -105 oC.