Table 2 Governing equations’ parameters

From: Microfluidic 3D cell culture: potential application of collagen hydrogels with an optimal dose of bioactive glasses

Parameter

Value

Ref

Density of media (water)

1000 kg/m3

43

Dynamic viscosity of media (water)

1 mPa × s

43

Density of collagen solution (2.0 mg/mL)

1000 kg/m3

44

Dynamic viscosity of collagen solution (2.0 mg/mL)

6 mPa × s

45

Collagen solution velocity at the inlet

50 µm/s

45

Diffusion coefficient for a 10 kDa dextran molecule within media at 37 °C

9.25 × 10–11 m2/s

46

Diffusion coefficient for a 10 kDa dextran molecule within the 3D collagen type I gel (2.0 mg/mL)

8.7 × 10–11 m2/s

46

Permeability coefficient in the collagen type I gel (porous media)

0.25 × 10–15 m2

47

Porosity of collagen type I gel

0.40

47

Contact angle between the liquid interface and the side wall

140 × π/180

40

Surface tension of the gel channel

0.07 N/m

40