Table 4 Results of the specific surface area measurements.

From: Microstructure and phase evolution in increasing the amount of mo and Ti of non-equiatomic CoFeNi-based medium entropy alloys for organic wastewater treatment

Sample

BET, m2/g

BJH, m2/g

BET pore, nm

(CoFeNi)95Mo2Ti3

0.17

0.782

15.45

(CoFeNi)90Mo4Ti6

0.17

0.083

20.08

(CoFeNi)85Mo6Ti9

0.05

0.032

14.43

(CoFeNi)80Mo8Ti12

0.23

0.129

19.83

(CoFeNi)75Mo10Ti15

0.21

0.129

12.90

(CoFeNi)70Mo12Ti18

0.21

0.131

11.68