Fig. 6
From: The effect of artificial aging after multi-directional forging of supersaturated AA2024

Comparison of SEM images and elemental analysis maps of 2024 aluminum alloy solution samples at 500 °C for 1 h, after MDF (single pass) and aged at (a) 100 °C, (b) 140 °C for 1 h and EDS corresponding to the area marked in figure (a, b).