Fig. 7
From: The effect of artificial aging after multi-directional forging of supersaturated AA2024

FE-SEM images of aluminum alloy 2024 dissolved samples at 500 ℃ for 1 h, post-MDF (single pass) and aged at (a) 190 ℃, (b) 240 ℃, (c) 290 ℃ for 1 h and EDS Corresponding to the area marked in Figure (b).