Fig. 8
From: The effect of artificial aging after multi-directional forging of supersaturated AA2024

EDS and elemental analysis maps of intermetallic particles of 2024 aluminum alloy solution samples at 500℃ for 1 h, post-MDF (single pass) and aged at 240℃ for 1 h.