Fig. 22

Internal microstructure of SLM Ti6Al4V after nitriding at 1050 °C, 15 min. (a) SEM microstructure of S13 sample nitrided in SF; (b) SEM microstructure of S18 sample nitrided in EF.
Internal microstructure of SLM Ti6Al4V after nitriding at 1050 °C, 15 min. (a) SEM microstructure of S13 sample nitrided in SF; (b) SEM microstructure of S18 sample nitrided in EF.