Fig. 37

Microhardness profile of samples of SLM Ti6Al4V nitrided for 10 min. at 900 °C, 1050 °C, and 1200 °C in solar furnace (a) and electric furnace (b).
Microhardness profile of samples of SLM Ti6Al4V nitrided for 10 min. at 900 °C, 1050 °C, and 1200 °C in solar furnace (a) and electric furnace (b).