Table 3 XPS survey scan composition of Li+-loaded resin 11.

From: Synthesis of a cross-linked polymer using a diallylammonium monomer containing 12-crown-4 motifs for the selective extraction of lithium ions

Name

Peak BE

FWHM eV

Atomic %

C1s A

285.87

2.28

64.94

C1s B

286.72

0.83

23.6

O1s A

530.59

1.73

0.79

O1s B

532.85

2.56

8.45

O1s C

532.43

1.63

15.07

N1s A

399.25

1.48

2.63

N1s B

401.81

2.33

1.43

S2p3 A

168.26

1.8

3.35

S2p1 A

169.32

1.8

1.64