Fig. 4

SEM micrographs of: (a) pure PVA, (b) S1 (low ZTO content), and inset dimension of the aggregates. (c) S2 (moderate ZTO content), and (d) S3 (high ZTO content). Increasing ZTO concentration leads to higher surface roughness and more pronounced nanoparticle agglomeration.