Fig. 2

Macroscopic morphology of fabricated PCL/gelatin scaffolds with varying polymer ratios (50:50, 60:40, and 70:30) and centrifugal conditions (5000 and 10,000 rpm for 5 and 10 min).

Macroscopic morphology of fabricated PCL/gelatin scaffolds with varying polymer ratios (50:50, 60:40, and 70:30) and centrifugal conditions (5000 and 10,000 rpm for 5 and 10 min).