Table 4 The storage modulus (E’), glass transition temperature (Tg) and maximum loss factor (tan δmax) of SBR composites.
Sample | (E’) @ 25 °C | Tg (°C) | tanδmax |
---|---|---|---|
S0/50C | 18.8 | -37.4 | 0.71 |
S10/40C | 17.0 | -41.1 | 0.69 |
S20/30C | 17.9 | -44.8 | 0.68 |
S30/20C | 15.3 | -42.3 | 0.63 |
S40/10C | 12.6 | -49.7 | 0.64 |
S50/0C | 11.3 | -55.5 | 0.52 |