Table 7 Orthogonal test results.
From: Study on the performance and mechanism of graphene oxide / polyurethane composite modified asphalt
Test number | Evaluation | |||
---|---|---|---|---|
Penetration(0.1 mm) | Softening point(℃) | 5℃ ductility(cm) | Elastic recovery(%) | |
1 | 53.6 | 64.1 | 8.0 | 83.4 |
2 | 50.5 | 70.3 | 8.2 | 85.2 |
3 | 48.9 | 67.8 | 7.7 | 84.4 |
4 | 47.3 | 69.1 | 7.5 | 85.6 |
5 | 49.7 | 62.9 | 8.3 | 82.4 |
6 | 53.8 | 71.8 | 7.9 | 84.9 |
7 | 44.5 | 68.0 | 8.5 | 82.7 |
8 | 47.6 | 67.7 | 8.8 | 86.4 |
9 | 50.8 | 72.9 | 8.1 | 80.7 |
10 | 48.1 | 76.5 | 9.2 | 82.5 |
11 | 44.5 | 62.3 | 8.1 | 80.6 |
12 | 47.2 | 75.2 | 8.7 | 82.1 |
13 | 53.9 | 61.2 | 9.1 | 83.2 |
14 | 50.1 | 66.3 | 8.4 | 88.1 |
15 | 48.9 | 60.5 | 9.0 | 83.3 |
16 | 49.2 | 73.4 | 8.9 | 80.4 |