From: Observation of magnetic skyrmion lattice in Cr0.82Mn0.18Ge by small-angle neutron scattering

(a) Ring-like SANS pattern measured at 11 K and 12 mT (SkL phase) in the longitudinal-field geometry. (b) Six Bragg peaks from the ordered hexagonal SkL emerging in SANS after rotating the sample in field. (c) Azimuthal distribution of the radially integrated SANS intensity after different rotation cycles.