Table 2 Grain size data for the AA and processed AZ31 billets. All units are in µm.

From: Corrosion and degradation behavior of MCSTE-Processed AZ31 magnesium alloy

 

AA

4P-30

8P-30

1P-40

2P-40

Min

5.05

2.52

2.26

1.35

1.17

Max

76.90

64.33

57.23

52.13

68.46

Average

22.18

7.60

6.25

5.96

5.41

Standard Deviation

14.78

7.37

5.95

7.48

7.51