Fig. 8

(a) Cycling performances and coulombic efficiency of Gr/Li half cells in STD and STD + Mg at 1 C after 500 cycles between 0 and 1.5 V; (b) EIS spectra of Gr/Li cells in the two electrolytes after 100 cycles at 2 C; (c) Cycling performances and coulombic efficiency of LNMO/Gr full cells in the two electrolytes after 100 cycles at 0.5 C between 3.5 and 4.9 V; (d) The galvanostatic charge/discharge curves of LNMO/Gr full cells in STD and STD + Mg electrolytes in the 1st and 100th cycles; (e) XRD patterns of LNMO cathodes disassembled from LNMO/Gr full cells in the two electrolytes after 100 cycles at 0.5 C; (f) XRD patterns of Gr anodes disassembled from LNMO/Gr full cells in in the two electrolytes after 100 cycles at 0.5 C.