Fig. 4

Raman intensity with the characteristic G peak of graphene in the insets (left) and the usual baseline-corrected spectra (right) of GQD multilayer colloidal crystal samples, synthesized with the experimental parameters listed in Table 1. Here, the curve color of two-kind Raman intensities is the same for an individual sample in Table 1.