Fig. 5

The full reflectance in the top row of the colloidal crystals synthesized with the parameters in Table 1. Here, high- and low-energy, UV-IR peaks are pointed out by color big arrows. The curve color is the same for an individual sample as Raman intensity in Fig. 4. The color dotted lines in the middle row are the result of the deconvolution of the peaks. In the bottom row, FWHMs are plotted as the function of GQD rate, the diameter of PS@GQDs and the 3 M template layer, with the curve colors are the same as the arrow colors in the same column.