Table 2 XRD data, d-spacing, graphitisation degree parameter, and crystallite size of catalyst-doped samples pyrolysed at 900 °C.
From: The facile conversion of waste biomass into few-layer graphene oxide
Sample name | 2 Theta (degree) | d-spacing (Å) | Graphitisation degree | FWHM | Crystallite size (nm) |
---|---|---|---|---|---|
4D | 28.8 | 0.309 | 0.398 | 0.20675 | 6.923887 |
4C | 28.67 | 0.311 | 0.382 | 34.6696 | 0.041278 |
3D | 29.11 | 0.307 | 0.436 | – | – |
3C | 29.08 | 0.306 | 0.432 | 0.26766 | 5.351627 |
2D | 29.19 | 0.305 | 0.445 | 0.26811 | 5.343978 |