Table 3 XRD data, d-spacing, graphitisation degree parameter, and crystallite size of low catalyst samples pyrolysed at 950 °C.

From: The facile conversion of waste biomass into few-layer graphene oxide

Sample name

2 Theta (degree)

d spacing (Å)

Graphitisation degree (%)

FWHM

Crystallite size (nm)

1C

25.66

3.47

0.92

100

1D

25.59

3.45

1.12

62

2C

26.20

3.39

58.12

0.75

96

2D

26.33

3.38

69.77

1.12

62