Fig. 7

A and B) Capacitance retention GCD profiles of Pure PPy MPC and PPy-CoO MPC at flat and bending positions at different angles after 10,000 cycles.
A and B) Capacitance retention GCD profiles of Pure PPy MPC and PPy-CoO MPC at flat and bending positions at different angles after 10,000 cycles.