Table 2 Equivalent circuit fitting parameters of uncoated and coated platinum before, and uncoated platinum after stimulation at varying current levels.
From: Endovascular neural stimulation with platinum and platinum black modified electrodes
Electrode | Stimulation | R1 /Ω | Q0 /10− 7 S s1/2 | n | R2 /kΩ | χ2 |
---|---|---|---|---|---|---|
Uncoated | Pre | 598 (114) | 9.7 (3.6) | 0.82 (0.03) | 349 (104) | 0.029 |
Uncoated | 0% | 537 (25) | 13.1 (2.7) | 0.76 (0.03) | 320 (19) | 0.021 |
Uncoated | 50% | 414 (26) | 23.3 (3.5) | 0.73 (0.03) | 223 (51) | 0.027 |
Uncoated | 90% | 562 (157) | 10.0 (2.8) | 0.80 (0.01) | 256 (34) | 0.024 |
Coated | Pre | 568 (135) | 63.7 (3.7) | 0.85 (0.01) | 827 (537) | 0.035 |