Table 1 Chemical composition of the used materials: GGBS, WGP, and DK.

From: Experimental and numerical evaluation of the mechanical behavior of alkali-activated slag concrete with recycled waste glass and dealuminated metakaolin powders

Constituents (%)

GGBFS

WGP

DK

SiO2

35.40

76.84

68.1

Al2O3

17.40

2.12

10.22

Fe2O3

1.40

0.5

0.65

CaO

36.87

5.23

0.59

MgO

7.83

3.29

0.1

MnO

0.18

0.03

0.01

Na2O

0.34

6.39

13.5

K2O

-

0.34

0.09

TiO2

0.38

0.16

2.74

SO3

0.2

1.62

2.55

L.O.I

-

2.89

1.15