Fig. 6: Labelled X-ray diffraction pattern of synthesized SnO platelets, alongside comparison to typical relative peak intensities for SnO powder (normalized by the integral signal intensity of the sample).
From: Solvent engineered synthesis of layered SnO for high-performance anodes

The normalized intensity is given with respect to the [101] peak. The asterisk indicates an equipment peak.