Fig. 6 | Communications Chemistry

Fig. 6

From: Voltage fade mitigation in the cationic dominant lithium-rich NCM cathode

Fig. 6

Understanding the chemical variation of LNCM1416 during the charge/discharge. a SQUID measurement of LNCM1416 displays the temperature-dependent inverse susceptibility at the applied field of 5000 Oe after discharging to 3.0, 3.75, 4.25, 4.5, and 4.55 voltages. b d-spacing versus voltage, displaying the variation of (001) interplanar spacing along the two cycles of charge/discharge, calculated from the operando XRD studies presented in the Supplementary Fig. 3