Fig. 8: Cycle life of NCM90505|LPSCl|Li/SS cells using different current collectors.

Cycle-life of a NCM90505|LPSCl|Li/SS cell, b NCM90505|LPSCl|Li/Ni cell, c NCM90505|LPSCl|Li/Cu cell, and d NCM90505|LPSCl|Li40/Cu (thickness of lithium on Cu foil is 40 μm) cell in a potential range of 2.7 and 4.3 V at room temperature at C/20 into coin cell format CR2032.