Fig. 5: Multifunctional performance of the SBE. | Communications Materials

Fig. 5: Multifunctional performance of the SBE.

From: Three-dimensional reconstruction and computational analysis of a structural battery composite electrolyte

Fig. 5

Storage modulus and ionic conductivity of SBE. a Storage modulus measured by DMA for the bulk polymer and SBE. b Nyquist plot of EIS data for the SBE. c 20 SVEs were extracted from the 3D reconstructed model. Two SVEs of d the polymer and e the liquid electrolyte domains, respectively. The geometries are slightly defeatured for FEM simulation. The geometric dimensions of the SVEs are 1.18 × 1.22 × 1.18 μm3. FEM simulation results from all SVEs for f elastic modulus and g ionic conductivity. Each data point corresponds to one SVE simulation; the red dot represents the final average result.

Back to article page