Table 1 Sulfur mass loading and electrolyte to sulfur ratios of the PVDF and carrageenan containing electrodes
From: Improving lithium-sulfur battery performance using a polysaccharide binder derived from red algae
Sample | Short name | Composition | Sulfur mass loading (mg) | E to S ratio (μL·mg−1) |
---|---|---|---|---|
S60SP30PVDF10 | PVDF10 | 60 wt.% S, 30 wt.% SuperP, 10 wt.% PVDF | 1.10 | 18.18 |
S60SP35CARR5 | CARR5 | 60 wt.% S, 35 wt.% SuperP, 5 wt.% Carr | 1.10 | 18.18 |
S63SP30CARR7 | CARR7 | 63 wt.% S, 30 wt.% SuperP, 6 wt.% Carr | 1.82 | 10.99 |
S60SP30CARR10 | CARR10 | 60 wt.% S, 30 wt.% SuperP, 10 wt.% Carr | 1.65 | 12.12 |
S70SP15CARR15 | CARR15 | 70 wt.% S, 15 wt.% SuperP, 15 wt.% Carr | 2.23 | 8.97 |
S70SP20CARR10 | CARR10b | 70 wt.% S, 20 wt.% SuperP, 10 wt.% Carr | 1.86 | 10.75 |